全部文献期刊会议图书|学者科研项目
中外文文献  中文文献  外文文献
作者:N. N. Popova , N. I. Sandler , N. I. Butko
来源:[J].Metal Science and Heat Treatment(IF 0.162), 1966, Vol.7 (11), pp.723-724
摘要:... The critical embrittlement temperature decreases from −30 to −40°Cto −60 to −70°C.(#br) 3. The sensitivity to stress concentrations and the resistence to mechanical aging, and also the weldability and the resistence of welds to vibrations in MSt. 3 steel are th...
作者:J.H. Bulloch
来源:[J].International Journal of Pressure Vessels and Piping(IF 0.932), 1999, Vol.76 (2), pp.63-78
摘要:Abstract(#br)This article describes a large in-service embrittlement study concerning six separate series of steam turbine casing bolts involving nearly four hundred individual bolts. The bolts, which ranged in size from 300 to 1400 mm in length, were fabricated from low alloy ...
作者:SV Brahimi , KR Sriraman , S Yue
来源:[J].Proceedings of the Institution of Mechanical Engineers(IF 0.633), 2017, Vol.231 (17), pp.3214-3227
摘要:Hydrogen embrittlement threshold curves were derived for two quenched and tempered steel grades, AISI 4135 and AISI 4340, at varying hardness ranging from 33 to 54 HRC. For each material, hydrogen was introduced (i) by zinc electroplating as a worst case condition for internal hy...
作者:Yu. Ya. Meshkov, S. O. Kotrechko, A. V. Shiyan
来源:[J].Metallofiz. Noveishie Tekhnol.(IF 0.108), 2019, Vol.41 (5), pp.633-646
摘要:... Using the results of testing samples with circumferential notches for uniaxial tension, the threshold values of a special indicator of reserve properties of strength and ductility of steels—deformation endurance (break resistance) $B_{rb}$ are determined. Below these val...
作者:SV Brahimi , KR Sriraman , S Yue
来源:[J].Proceedings of the Institution of Mechanical Engineers, Part C: Journal of Mechanical Engineering Science(IF 0.633), 2017, Vol.231 (17), pp.3214-3227
摘要:Hydrogen embrittlement threshold curves were derived for two quenched and tempered steel grades, AISI 4135 and AISI 4340, at varying hardness ranging from 33 to 54 HRC. For each material, hydrogen was introduced (i) by zinc electroplating as a worst case condition for internal...